Customization: | Available |
---|---|
Material: | St6(Cobalt Alloy) |
Application: | Railroad Weld Removal Machine |
Still deciding? Get samples of US$ 50/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Cobalt alloy steam corrosion shields are welded to steam turbine blades. Cobalt alloys have high hardness and toughness, slight variation when water droplets hit, good resistance to water corrosion and erosion, and high microstructure stability, although beyond a particular range. Water corrosion will also occur, but the ability to resist fracture is good, and even if severe water corrosion occurs, it is not easy to produce cracks. At the same time, different alloy shapes can be selected according to the operating conditions. When the water corrosion is severe, a new cobalt alloy sheet can be replaced, which is very suitable for the working conditions of the blade. Therefore, when welding cobalt alloy, the most commonly used method to prevent water corrosion of steam turbine blades is
Chemical compositions and properties (%)
Brand |
C |
Mn |
Si |
Cr |
Ni |
Mo |
W |
Co |
Fe |
P |
S |
Density (g/cm3) |
Hardness (HRC) |
Co 3 |
2.0-2.7 |
1.0 |
1.0 |
29-33 |
3.0 |
|
11-14 |
Bal. |
3.0 |
≤0.03 |
≤0.03 |
8.55 |
51-55 |
Co 6 |
0.9-1.4 |
1.0 |
1.5 |
27-31 |
3.0 |
1.5 |
3.5-5.5 |
Bal. |
3.0 |
≤0.03 |
≤0.03 |
8.35 |
38-44 |
Co 12 |
1.1-1.7 |
1.0 |
1.0 |
28-32 |
3.0 |
|
7.0-9.5 |
Bal. |
3.0 |
≤0.03 |
≤0.03 |
8.40 |
44-49 |
Co 20 |
2.2-3.0 |
|
2.0 |
30-34 |
3.0 |
1.0 |
14-18 |
Bal. |
3.0 |
≤0.05 |
≤0.05 |
8.65 |
53-59 |
T400 |
0.04 |
|
2.5-2.7 |
8-10 |
|
27-29 |
|
Bal. |
|
|
|
|
55 |
T800 |
0.04 |
|
3.2-3.6 |
16-18 |
|
27-29 |
|
Bal. |
|
|
|
|
58 |
Q1: Are you a manufacturer or a trading company?
A1: We are a manufacturer located in the north of China with 15 years of producing experience and 10 years of exporting experience.
Q2: What's the material of your bushings/sleeves?
A2: It's the CoCrW alloy, usually called cobalt alloy.
Q3: What's the cobalt alloy?
A3: It is a range of cobalt-chromium alloys designed for wear resistance, heat resistance and corrosion resistance.
Q4: What's the lead time of bushings?
A4: 15-35 days, depending on the order quantity.
Q5: What's the tolerance and surface finish we can control?
A5: As your demand.
Q6: How do we deliver the seats?
A6: We are a VIP customer of DHL Express with good discounts.
Q7: MOQ?
A7: According to different products, there will be different MOQs, but a 1pc sample is acceptable