Customization: | Available |
---|---|
Customized: | Customized |
Material: | Cobalt Alloy |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Cobalt chrome plate
1. Cobalt alloys have higher melting points than nickel (or iron) alloys, Which allows them to absorb stress at a higher absolute temperature.
2. Cobalt alloys give superior hot corrosion resistance to gas turbine atmospheres due to their high chromium content.
3. Cobalt alloys show superior thermal fatigue resistance and weldability over nickel alloys.
---Excellent wear and corrosion resistance even at high temperatures up to 800
SYTOP cobalt base alloys is a range of cobalt-chromium-tungsten alloys with wear resistance, corrosion and high thermal resistance. It is widely used in oil & gas, machinery, wood cutting, automotive, paper and food processing industry, etc.
Chemical compositions and properties (%)
Brand |
C |
Mn |
Si |
Cr |
Ni |
Mo |
W |
Co |
Fe |
P |
S |
Density (g/cm3) |
Hardness (HRC) |
Co 3 |
2.0-2.7 |
1.0 |
1.0 |
29-33 |
3.0 |
11-14 |
Bal. |
3.0 |
≤0.03 |
≤0.03 |
8.55 |
51-55 |
|
Co 6 |
0.9-1.4 |
1.0 |
1.5 |
27-31 |
3.0 |
1.5 |
3.5-5.5 |
Bal. |
3.0 |
≤0.03 |
≤0.03 |
8.35 |
38-44 |
Co 12 |
1.1-1.7 |
1.0 |
1.0 |
28-32 |
3.0 |
7.0-9.5 |
Bal. |
3.0 |
≤0.03 |
≤0.03 |
8.40 |
44-49 |
|
Co 20 |
2.2-3.0 |
2.0 |
30-34 |
3.0 |
1.0 |
14-18 |
Bal. |
3.0 |
≤0.05 |
≤0.05 |
8.65 |
53-59 |
|
Co 400 |
0.04 |
2.5-2.7 |
8-10 |
27-29 |
Bal. |
55 |
|||||||
Co 800 |
0.04 |
3.2-3.6 |
16-18 |
27-29 |
Bal. |
58 |